Titanium alloy workpiece burr processing method!

Release time:2021-11-03 22:25:29 丨 Number of visits:

This mechanical treatment method is: titanium material buried in a lot of abrasives, adding some grinding and polishing compounds dissolved in water, using the principle of oscillation to mix abrasives with data, constantly requiring the workpiece cleaning, grinding the surface and corners of the workpiece with abrasives, and then polishing. The technology can be used for deburring, chamfering, rust removal, descaling, smooth polishing of metal parts of various sizes and shapes.


Abrasives can be alumina (including molten, sintered or natural), corundum, plastics, timely, ceramic, etc. And can be single or a mixture of several. These abrasives can be made into dihedral angles, cylinders, diamonds, etc. They were made into prefabricated abrasives in the first place because they are more economical and faster than any shape and natural shape data. According to the shape and size of the workpiece, choose different shapes and sizes of abrasives. Abrasive materials used for rolling include pumice stone, timing, granite horns, shells, iron shavings, and ceramic shards. The abrasive size should be larger or smaller than each hole of the part. The quantity of contents in the drum is also an important factor affecting the quality of agricultural parts. The number of people in the drum usually accounts for 70% of the volume of the drum. The amount of solution added in the roller should account for about 95% of the volume of the roller (note: when adding acidic solution in the roller, add enough water first, and then add acid, so as not to corrosion parts in the rolling process. With the increase of time, the concentration of the solution in the drum gradually decreases and even loses its effect.


The processing time can vary from a few minutes to several hours. The key is to choose abrasive material, which is determined through experiments. Only in this way can we get a uniform and bright appearance. After processing, the workpiece is discharged together with the abrasive and taken out after screening by the separator. The recycled abrasive can continue to return to processing. Swing finishing machine is divided into single machine and online two types, according to the production demand choice.



Contact Us


Baoji Hengyuxin Metal Co., Ltd.
Tel:+86-0917-6735123
   +86-18740677522
E-mail:sales@hyxti.com
Add:No.168 Gaoya Village Industrial Zone,Bayu Town,Gaoxin Development District,Baoii,shaanxi.China
陕ICP备18004305号